Follow
Hiroshi Fujiwara
Hiroshi Fujiwara
Verified email at fc.ritsumei.ac.jp
Title
Cited by
Cited by
Year
New microstructure design for commercially pure titanium with outstanding mechanical properties by mechanical milling and hot roll sintering
T Sekiguchi, K Ono, H Fujiwara, K Ameyama
Materials transactions 51 (1), 39-45, 2010
1542010
Obtaining copper with harmonic structure for the optimal balance of structure-performance relationship
D Orlov, H Fujiwara, K Ameyama
Materials transactions 54 (9), 1549-1553, 2013
872013
Cold consolidation of ball-milled titanium powders using high-pressure torsion
K Edalati, Z Horita, H Fujiwara, K Ameyama
Metallurgical and Materials Transactions A 41, 3308-3317, 2010
782010
Nano-ferrite formation and strain-induced-ferrite transformation in an SUS316L austenitic stainless steel
H Fujiwara, H Inomoto, R Sanada, K Ameyama
Scripta materialia 44 (8-9), 2039-2042, 2001
682001
Enhanced mechanical properties of nano/meso hybrid structure materials produced by hot roll sintering process
H Fujiwara, R Akada, A Noro, Y Yoshita, K Ameyama
Materials transactions 49 (1), 90-96, 2008
632008
Corrosion behavior of severely deformed pure and single-phase materials
H Miyamoto, M Yuasa, M Rifai, H Fujiwara
Materials Transactions 60 (7), 1243-1255, 2019
552019
Effects of Strain Energy and Grain Size on Corrosion Resistance of Ultrafine Grained Fe‐20% Cr Steels with Extremely low C and N Fabricated by ECAP
M Rifai, H Miyamoto, H Fujiwara
International Journal of Corrosion 2015 (1), 386865, 2015
452015
Enhanced corrosion resistance of CoCrFeMnNi high entropy alloy using heterogeneous structure design
J Wang, Z Zhang, H Dai, H Fujiwara, X Chen, K Ameyama
Corrosion Science 209, 110761, 2022
442022
Mechanical properties of pure titanium and Ti-6Al-4V alloys with a new tailored nano/meso hybrid microstructure
H Fujiwara, T Sekiguchi, K Ameyama
International journal of materials research 100 (6), 796-799, 2009
422009
Preferred orientation relationship of intra-and inter-granular precipitates in titanium alloys
N Miyano, H Fujiwara, K Ameyama, GC Weatherly
Materials Science and Engineering: A 333 (1-2), 85-91, 2002
402002
Severe plastic deformation for producing Superfunctional ultrafine-grained and heterostructured materials: An interdisciplinary review
K Edalati, AQ Ahmed, S Akrami, K Ameyama, V Aptukov, RN Asfandiyarov, ...
Journal of Alloys and Compounds, 174667, 2024
332024
Creation of harmonic structure materials with outstanding mechanical properties
K Ameyama, F Hiroshi
Materials Science Forum 706, 9-16, 2012
332012
A microstructural aspect of intergranular stress corrosion cracking of semi-hard U-bend tubes of commercially pure copper in cooling systems
H Miyamoto, D Saburi, H Fujiwara
Engineering Failure Analysis 26, 108-119, 2012
322012
Nano grain formation in tungsten by severe plastic deformation-mechanical milling process
E Oda, H Fujiwara, K Ameyama
Materials transactions 49 (1), 54-57, 2008
312008
The effect of ECAP deformation route on microstructure, mechanical and electrochemical properties of low CN Fe-20% Cr alloy
M Rifai, H Miyamoto, H Fujiwara
Materials Sciences and Applications 5 (8), 568-578, 2014
282014
“Special” to “general” transition of intergranular corrosion in Σ3 {1 1 1} grain boundary with gradually changed misorientation
Y Takehara, H Fujiwara, H Miyamoto
Corrosion science 77, 171-175, 2013
272013
Mechanical properties of harmonic structured composite with pure titanium and Ti–48 at% Al alloy by MM/SPS process
H Fujiwara, T Kawabata, H Miyamoto, K Ameyama
Materials Transactions 54 (9), 1619-1623, 2013
232013
Nano-Grain formation in a fully Ferritic Sus 316L austenitic stainless steel produced by Hs-Pm process
H Fujiwara, K Ameyama
Materials science forum 304, 47-52, 1999
231999
Microstructure and mechanical property of nano-duplex materials produced by HRS process
F Hiroshi, R Akada, Y Yoshita, K Ameyama
Materials Science Forum 503, 227-232, 2006
222006
Age-hardening mechanism for nanocrystalline Ni–P alloys synthesized by electrodeposition
Y Kasazaki, H Fujiwara, H Miyamoto
Surface and Coatings Technology 253, 154-160, 2014
202014
The system can't perform the operation now. Try again later.